Every forging shop knows the look of a part that came out of the die covered in oxide pits. The die filled, the dimensions are within tolerance, and the part still goes to the grinding bench. The cause was set earlier in the shift, at the furnace.
Scale forms with time and air. Oxide grows quickly once the billet surface enters the high-temperature range, and it grows with every extra minute at temperature and every unnecessary furnace door opening. A furnace run on a stable charge schedule produces a thinner scale layer than the same furnace run hot with billets waiting inside.
Heating practice comes first. Zone settings, soak time and the charge schedule decide how thick the scale layer will be. Two habits are worth enforcing: do not charge billets earlier than the pressing sequence needs, and record the actual time in and out for each charge. A billet that sits forty extra minutes arrives at the press with a different skin than the process was tuned for.
Remove what has formed. Where part quality requires it, descaling between furnace and die — high-pressure water or mechanical descaling — takes the loose layer off before it can be forged into the surface. Scale pressed into the face becomes pitting; scale left in a deep cavity becomes a filling problem, because the oxide occupies volume the metal needs.
Keep scale out of the die. Even with good heating, some oxide will fall into the die during handling. Blow air through the die before each billet and include the die face in the spray cycle. A servo screw press runs a programmable cycle, so the blow-off and spray steps can be timed against the press sequence rather than left to operator memory; site material on forging automation describes spray and handling devices working in step with the press cycle (public site material).
Inspect with a method. Surface defects concentrate in predictable places: deep cavities, web areas and corner radii. Check those zones first on the first article of every batch, and log what you find next to the heating record of that charge.
Surface quality is decided before the first blow. The furnace and the descaling step set the ceiling; the press can deliver what the billet surface allows.
References